Sintered NdFeB magnet N44H
N44H
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N44H (Eclipse Magnetics grade table): Br >= 1.33 T, HcJ >= 1353 kA/m, (BH)max >= 334 kJ/m^3 (minimum values), maximum operating temperature about 120 °C.
NdFeB N44H
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N46H
N46H
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N46H (Eclipse Magnetics grade table): Br >= 1.36 T, HcJ >= 1353 kA/m, (BH)max >= 350 kJ/m^3 (minimum values), maximum operating temperature about 120 °C.
NdFeB N46H
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N48H
N48H
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N48H (Eclipse Magnetics grade table): Br >= 1.38 T, HcJ >= 1353 kA/m, (BH)max >= 366 kJ/m^3 (minimum values), maximum operating temperature about 120 °C.
NdFeB N48H
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N30SH
N30SH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N30SH (Eclipse Magnetics grade table): Br >= 1.08 T, HcJ >= 1592 kA/m, (BH)max >= 223 kJ/m^3 (minimum values), maximum operating temperature about 150 °C.
NdFeB N30SH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N33SH
N33SH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N33SH (Eclipse Magnetics grade table): Br >= 1.14 T, HcJ >= 1592 kA/m, (BH)max >= 239 kJ/m^3 (minimum values), maximum operating temperature about 150 °C.
NdFeB N33SH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N35SH
N35SH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N35SH (Eclipse Magnetics grade table): Br >= 1.17 T, HcJ >= 1592 kA/m, (BH)max >= 263 kJ/m^3 (minimum values), maximum operating temperature about 150 °C.
NdFeB N35SH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N38SH
N38SH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N38SH (Eclipse Magnetics grade table): Br >= 1.22 T, HcJ >= 1592 kA/m, (BH)max >= 279 kJ/m^3 (minimum values), maximum operating temperature about 150 °C.
NdFeB N38SH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N40SH
N40SH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N40SH (Eclipse Magnetics grade table): Br >= 1.26 T, HcJ >= 1592 kA/m, (BH)max >= 303 kJ/m^3 (minimum values), maximum operating temperature about 150 °C.
NdFeB N40SH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N42SH
N42SH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N42SH (Eclipse Magnetics grade table): Br >= 1.30 T, HcJ >= 1592 kA/m, (BH)max >= 318 kJ/m^3 (minimum values), maximum operating temperature about 150 °C.
NdFeB N42SH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N44SH
N44SH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N44SH (Eclipse Magnetics grade table): Br >= 1.33 T, HcJ >= 1592 kA/m, (BH)max >= 334 kJ/m^3 (minimum values), maximum operating temperature about 150 °C.
NdFeB N44SH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N46SH
N46SH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N46SH (Eclipse Magnetics grade table): Br >= 1.36 T, HcJ >= 1592 kA/m, (BH)max >= 350 kJ/m^3 (minimum values), maximum operating temperature about 150 °C.
NdFeB N46SH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N28UH
N28UH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N28UH (Eclipse Magnetics grade table): Br >= 1.04 T, HcJ >= 1989 kA/m, (BH)max >= 199 kJ/m^3 (minimum values), maximum operating temperature about 180 °C.
NdFeB N28UH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N30UH
N30UH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N30UH (Eclipse Magnetics grade table): Br >= 1.08 T, HcJ >= 1989 kA/m, (BH)max >= 223 kJ/m^3 (minimum values), maximum operating temperature about 180 °C.
NdFeB N30UH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N33UH
N33UH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N33UH (Eclipse Magnetics grade table): Br >= 1.14 T, HcJ >= 1989 kA/m, (BH)max >= 239 kJ/m^3 (minimum values), maximum operating temperature about 180 °C.
NdFeB N33UH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N35UH
N35UH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N35UH (Eclipse Magnetics grade table): Br >= 1.17 T, HcJ >= 1989 kA/m, (BH)max >= 263 kJ/m^3 (minimum values), maximum operating temperature about 180 °C.
NdFeB N35UH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N38UH
N38UH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N38UH (Eclipse Magnetics grade table): Br >= 1.22 T, HcJ >= 1989 kA/m, (BH)max >= 279 kJ/m^3 (minimum values), maximum operating temperature about 180 °C.
NdFeB N38UH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N40UH
N40UH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N40UH (Eclipse Magnetics grade table): Br >= 1.26 T, HcJ >= 1989 kA/m, (BH)max >= 303 kJ/m^3 (minimum values), maximum operating temperature about 180 °C.
NdFeB N40UH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N28EH
N28EH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N28EH (Eclipse Magnetics grade table): Br >= 1.04 T, HcJ >= 2387 kA/m, (BH)max >= 199 kJ/m^3 (minimum values), maximum operating temperature about 200 °C.
NdFeB N28EH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N30EH
N30EH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N30EH (Eclipse Magnetics grade table): Br >= 1.08 T, HcJ >= 2387 kA/m, (BH)max >= 223 kJ/m^3 (minimum values), maximum operating temperature about 200 °C.
NdFeB N30EH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N33EH
N33EH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N33EH (Eclipse Magnetics grade table): Br >= 1.14 T, HcJ >= 2387 kA/m, (BH)max >= 239 kJ/m^3 (minimum values), maximum operating temperature about 200 °C.
NdFeB N33EH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N35EH
N35EH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N35EH (Eclipse Magnetics grade table): Br >= 1.17 T, HcJ >= 2387 kA/m, (BH)max >= 263 kJ/m^3 (minimum values), maximum operating temperature about 200 °C.
NdFeB N35EH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N38EH
N38EH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N38EH (Eclipse Magnetics grade table): Br >= 1.22 T, HcJ >= 2387 kA/m, (BH)max >= 279 kJ/m^3 (minimum values), maximum operating temperature about 200 °C.
NdFeB N38EH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N25AH
N25AH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N25AH (Eclipse Magnetics grade table): Br >= 0.97 T, HcJ >= 2787 kA/m, (BH)max >= 180 kJ/m^3 (minimum values), maximum operating temperature about 220 °C.
NdFeB N25AH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N28AH
N28AH
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N28AH (Eclipse Magnetics grade table): Br >= 1.04 T, HcJ >= 2787 kA/m, (BH)max >= 203 kJ/m^3 (minimum values), maximum operating temperature about 220 °C.
NdFeB N28AH
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.