Steel X2CrMoTi18-2
X2CrMoTi18-2
ДСТУ EN 10088-1:2019
ДСТУ EN 10088-2:2022
EN 10088-1:2014
EN 10088-2:2014
Ferrous metals
Molybdenum-alloyed titanium stabilized ferritic stainless steel with pitting resistance near the molybdenum austenitic grades, without nickel, for hot water tanks, heat exchanger tubes, roofing and kitchen equipment.
X2CrMoTi18-2
1.4521
Corrosion-resistant parts
Sheet metal parts
Welded structures
Pipes and tubes
Properties, analogues, sources, notes and hardness need a paid account.
Steel X12CrS13
X12CrS13
ДСТУ EN 10088-1:2019
ДСТУ EN 10088-3:2022
EN 10088-1:2014
EN 10088-3:2014
Ferrous metals
Free-machining sulphur-alloyed martensitic 13 % chromium stainless steel for turned parts, screws, nuts, valve and pump parts made on automatic lathes.
X12CrS13
1.4005
Corrosion-resistant parts
Turned parts
Fasteners
Shafts and axles
Properties, analogues, sources, notes and hardness need a paid account.
Steel X90CrMoV18
X90CrMoV18
ДСТУ EN 10088-1:2019
ДСТУ EN 10088-3:2022
EN 10088-1:2014
EN 10088-3:2014
Ferrous metals
High-carbon martensitic chromium-molybdenum-vanadium stainless steel hardened for knives, cutting blades, surgical tools, bearings and wear parts.
X90CrMoV18
1.4112
Corrosion-resistant parts
Cutting tools
Rolling bearings
Wear parts
Properties, analogues, sources, notes and hardness need a paid account.
Steel 12Kh13
12Х13
ГОСТ 5632-2014
ГОСТ 5949-75
ГОСТ 5582-75
ГОСТ 7350-77
Ferrous metals
GOST low-carbon martensitic 13 % chromium stainless steel for quenched and tempered valve, pump and turbine parts, fasteners and parts in water and steam.
12Х13
12X13
12Kh13
1Х13
Corrosion-resistant parts
Shafts and axles
Fasteners
Sheet metal parts
Properties, analogues, sources, notes and hardness need a paid account.
Steel 08Kh22N6T
08Х22Н6Т
ГОСТ 5632-2014
ГОСТ 5949-75
ГОСТ 5582-75
ГОСТ 7350-77
Ferrous metals
GOST austenitic-ferritic titanium-stabilized chromium-nickel stainless steel with less nickel than 18-10 grades for welded chemical apparatus, heat exchangers and pipes.
08Х22Н6Т
08X22H6T
08Kh22N6T
ЭП53
Corrosion-resistant parts
Welded structures
Pipes and tubes
Pressure vessels and boilers
Properties, analogues, sources, notes and hardness need a paid account.
Sintered isotropic hard ferrite 8/22
Hard ferrite 8/22
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered isotropic hard ferrite (strontium or barium hexaferrite) of EN 60404-8-1: Br >= 210 mT, HcJ >= 220 kA/m, (BH)max >= 8 kJ/m^3, operating temperature up to 250 °C; an isotropic magnet can be magnetized in any direction.
HF 8/22
Hartferrit 8/22
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered isotropic barium ferrite 6БИ240
6БИ240
ГОСТ 24063-80
Permanent magnets
Sintered isotropic barium hexaferrite magnet of ГОСТ 24063-80: Br >= 0.19 T, HcJ >= 240 kA/m, (BH)max >= 6 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered anisotropic barium ferrite 16БА190
16БА190
ГОСТ 24063-80
Permanent magnets
Sintered anisotropic barium hexaferrite magnet of ГОСТ 24063-80: Br >= 0.3 T, HcJ >= 190 kA/m, (BH)max >= 16 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered anisotropic barium ferrite 18БА220
18БА220
ГОСТ 24063-80
Permanent magnets
Sintered anisotropic barium hexaferrite magnet of ГОСТ 24063-80: Br >= 0.33 T, HcJ >= 220 kA/m, (BH)max >= 18 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered anisotropic barium ferrite 22БА220
22БА220
ГОСТ 24063-80
Permanent magnets
Sintered anisotropic barium hexaferrite magnet of ГОСТ 24063-80: Br >= 0.36 T, HcJ >= 220 kA/m, (BH)max >= 22 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered anisotropic barium ferrite 25БА150
25БА150
ГОСТ 24063-80
Permanent magnets
Sintered anisotropic barium hexaferrite magnet of ГОСТ 24063-80: Br >= 0.38 T, HcJ >= 150 kA/m, (BH)max >= 25 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered samarium-cobalt magnet КС37
КС37
ГОСТ 21559-76
Permanent magnets
Sintered hard magnetic material КС37 of ГОСТ 21559-76, SmCo5 type (samarium 35-39 %, cobalt rest): Br >= 0.77 T, HcB >= 540 kA/m, HcJ >= 1300 kA/m, (BH)max >= 110 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered samarium-cobalt magnet КС37А
КС37А
ГОСТ 21559-76
Permanent magnets
Sintered hard magnetic material КС37А of ГОСТ 21559-76, SmCo5 type (samarium 35-39 %, cobalt rest): Br >= 0.82 T, HcB >= 560 kA/m, HcJ >= 1000 kA/m, (BH)max >= 130 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered samarium-cobalt magnet КС36А
КС36А
ГОСТ 21559-76
Permanent magnets
Sintered hard magnetic material КС36А of ГОСТ 21559-76, SmCo5 type (samarium 35-39 %, cobalt rest): Br >= 0.9 T, HcB >= 660 kA/m, HcJ >= 900 kA/m, (BH)max >= 160 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered samarium-cobalt magnet КС25ДЦ-150
КС25ДЦ-150
ГОСТ 21559-76
Permanent magnets
Sintered hard magnetic material КС25ДЦ-150 of ГОСТ 21559-76, Sm2Co17 type (samarium 24-27 %, zirconium 1.5-3.5 %, iron 13-20 %, copper 4-9 %, cobalt rest): Br >= 0.9 T, HcB >= 690 kA/m, HcJ >= 900 kA/m, (BH)max >= 150 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered samarium-cobalt magnet КС25ДЦ-175
КС25ДЦ-175
ГОСТ 21559-76
Permanent magnets
Sintered hard magnetic material КС25ДЦ-175 of ГОСТ 21559-76, Sm2Co17 type (samarium 24-27 %, zirconium 1.5-3.5 %, iron 13-20 %, copper 4-9 %, cobalt rest): Br >= 0.94 T, HcB >= 700 kA/m, HcJ >= 900 kA/m, (BH)max >= 175 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered samarium-cobalt magnet КС25ДЦ-190
КС25ДЦ-190
ГОСТ 21559-76
Permanent magnets
Sintered hard magnetic material КС25ДЦ-190 of ГОСТ 21559-76, Sm2Co17 type (samarium 24-27 %, zirconium 1.5-3.5 %, iron 13-20 %, copper 4-9 %, cobalt rest): Br >= 0.98 T, HcB >= 710 kA/m, HcJ >= 900 kA/m, (BH)max >= 190 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered samarium-cobalt magnet КС25ДЦ-210
КС25ДЦ-210
ГОСТ 21559-76
Permanent magnets
Sintered hard magnetic material КС25ДЦ-210 of ГОСТ 21559-76, Sm2Co17 type (samarium 24-27 %, zirconium 1.5-3.5 %, iron 13-20 %, copper 4-9 %, cobalt rest): Br >= 1.02 T, HcB >= 740 kA/m, HcJ >= 900 kA/m, (BH)max >= 210 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered samarium-cobalt magnet КС25ДЦ-225
КС25ДЦ-225
ГОСТ 21559-76
Permanent magnets
Sintered hard magnetic material КС25ДЦ-225 of ГОСТ 21559-76, Sm2Co17 type (samarium 24-27 %, zirconium 1.5-3.5 %, iron 13-20 %, copper 4-9 %, cobalt rest): Br >= 1.06 T, HcB >= 760 kA/m, HcJ >= 900 kA/m, (BH)max >= 225 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered samarium-cobalt magnet КС25ДЦ-240
КС25ДЦ-240
ГОСТ 21559-76
Permanent magnets
Sintered hard magnetic material КС25ДЦ-240 of ГОСТ 21559-76, Sm2Co17 type (samarium 24-27 %, zirconium 1.5-3.5 %, iron 13-20 %, copper 4-9 %, cobalt rest): Br >= 1.1 T, HcB >= 780 kA/m, HcJ >= 900 kA/m, (BH)max >= 240 kJ/m^3.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered isotropic AlNiCo magnet 8/4
AlNiCo 8/4
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered isotropic AlNiCo permanent magnet of EN 60404-8-1: Br 0.5 T, HcJ 40 kA/m, (BH)max 8 kJ/m^3, operating temperature up to 450 °C, temperature coefficient of Br -0.022 %/K.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered isotropic AlNiCo magnet 12/5
AlNiCo 12/5
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered isotropic AlNiCo permanent magnet of EN 60404-8-1: Br 0.64 T, HcJ 50 kA/m, (BH)max 12 kJ/m^3, operating temperature up to 450 °C, temperature coefficient of Br -0.014 %/K.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered isotropic AlNiCo magnet 18/8
AlNiCo 18/8
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered isotropic AlNiCo permanent magnet of EN 60404-8-1: Br 0.65 T, HcJ 82 kA/m, (BH)max 18 kJ/m^3, operating temperature up to 450 °C, temperature coefficient of Br -0.02 %/K.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered anisotropic AlNiCo magnet 28/6
AlNiCo 28/6
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic AlNiCo permanent magnet of EN 60404-8-1: Br 1 T, HcJ 58 kA/m, (BH)max 28 kJ/m^3, operating temperature up to 525 °C, temperature coefficient of Br -0.02 %/K.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.