Sintered NdFeB magnet VACODYM 776 TP
VACODYM 776 TP
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet VACODYM 776 TP (VACUUMSCHMELZE): Br 1.32 T, HcJ >= 1670 kA/m, (BH)max 335 kJ/m^3 (typical), maximum operating temperature about 140 °C.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet VACODYM 890 TP
VACODYM 890 TP
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet VACODYM 890 TP (VACUUMSCHMELZE): Br 1.19 T, HcJ >= 2625 kA/m, (BH)max 270 kJ/m^3 (typical), maximum operating temperature about 220 °C.
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N35
N35
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N35 (Eclipse Magnetics grade table): Br >= 1.17 T, HcJ >= 955 kA/m, (BH)max >= 263 kJ/m^3 (minimum values), maximum operating temperature about 80 °C.
NdFeB N35
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N38
N38
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N38 (Eclipse Magnetics grade table): Br >= 1.22 T, HcJ >= 955 kA/m, (BH)max >= 279 kJ/m^3 (minimum values), maximum operating temperature about 80 °C.
NdFeB N38
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N40
N40
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N40 (Eclipse Magnetics grade table): Br >= 1.26 T, HcJ >= 955 kA/m, (BH)max >= 303 kJ/m^3 (minimum values), maximum operating temperature about 80 °C.
NdFeB N40
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N42
N42
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N42 (Eclipse Magnetics grade table): Br >= 1.30 T, HcJ >= 955 kA/m, (BH)max >= 318 kJ/m^3 (minimum values), maximum operating temperature about 80 °C.
NdFeB N42
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N45
N45
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N45 (Eclipse Magnetics grade table): Br >= 1.33 T, HcJ >= 955 kA/m, (BH)max >= 334 kJ/m^3 (minimum values), maximum operating temperature about 80 °C.
NdFeB N45
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N48
N48
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N48 (Eclipse Magnetics grade table): Br >= 1.37 T, HcJ >= 955 kA/m, (BH)max >= 358 kJ/m^3 (minimum values), maximum operating temperature about 80 °C.
NdFeB N48
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N50
N50
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N50 (Eclipse Magnetics grade table): Br >= 1.41 T, HcJ >= 875 kA/m, (BH)max >= 382 kJ/m^3 (minimum values), maximum operating temperature about 70 °C.
NdFeB N50
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N52
N52
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N52 (Eclipse Magnetics grade table): Br >= 1.44 T, HcJ >= 875 kA/m, (BH)max >= 398 kJ/m^3 (minimum values), maximum operating temperature about 70 °C.
NdFeB N52
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N33M
N33M
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N33M (Eclipse Magnetics grade table): Br >= 1.14 T, HcJ >= 1114 kA/m, (BH)max >= 239 kJ/m^3 (minimum values), maximum operating temperature about 100 °C.
NdFeB N33M
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N35M
N35M
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N35M (Eclipse Magnetics grade table): Br >= 1.17 T, HcJ >= 1114 kA/m, (BH)max >= 263 kJ/m^3 (minimum values), maximum operating temperature about 100 °C.
NdFeB N35M
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N38M
N38M
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N38M (Eclipse Magnetics grade table): Br >= 1.22 T, HcJ >= 1114 kA/m, (BH)max >= 279 kJ/m^3 (minimum values), maximum operating temperature about 100 °C.
NdFeB N38M
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N40M
N40M
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N40M (Eclipse Magnetics grade table): Br >= 1.26 T, HcJ >= 1114 kA/m, (BH)max >= 303 kJ/m^3 (minimum values), maximum operating temperature about 100 °C.
NdFeB N40M
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N42M
N42M
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N42M (Eclipse Magnetics grade table): Br >= 1.30 T, HcJ >= 1114 kA/m, (BH)max >= 318 kJ/m^3 (minimum values), maximum operating temperature about 100 °C.
NdFeB N42M
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N45M
N45M
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N45M (Eclipse Magnetics grade table): Br >= 1.33 T, HcJ >= 1114 kA/m, (BH)max >= 334 kJ/m^3 (minimum values), maximum operating temperature about 100 °C.
NdFeB N45M
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N48M
N48M
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N48M (Eclipse Magnetics grade table): Br >= 1.37 T, HcJ >= 1114 kA/m, (BH)max >= 358 kJ/m^3 (minimum values), maximum operating temperature about 90 °C.
NdFeB N48M
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N50M
N50M
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N50M (Eclipse Magnetics grade table): Br >= 1.41 T, HcJ >= 1114 kA/m, (BH)max >= 382 kJ/m^3 (minimum values), maximum operating temperature about 90 °C.
NdFeB N50M
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N30H
N30H
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N30H (Eclipse Magnetics grade table): Br >= 1.08 T, HcJ >= 1353 kA/m, (BH)max >= 223 kJ/m^3 (minimum values), maximum operating temperature about 120 °C.
NdFeB N30H
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N33H
N33H
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N33H (Eclipse Magnetics grade table): Br >= 1.14 T, HcJ >= 1353 kA/m, (BH)max >= 239 kJ/m^3 (minimum values), maximum operating temperature about 120 °C.
NdFeB N33H
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N35H
N35H
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N35H (Eclipse Magnetics grade table): Br >= 1.17 T, HcJ >= 1353 kA/m, (BH)max >= 263 kJ/m^3 (minimum values), maximum operating temperature about 120 °C.
NdFeB N35H
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N38H
N38H
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N38H (Eclipse Magnetics grade table): Br >= 1.22 T, HcJ >= 1353 kA/m, (BH)max >= 279 kJ/m^3 (minimum values), maximum operating temperature about 120 °C.
NdFeB N38H
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N40H
N40H
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N40H (Eclipse Magnetics grade table): Br >= 1.26 T, HcJ >= 1353 kA/m, (BH)max >= 303 kJ/m^3 (minimum values), maximum operating temperature about 120 °C.
NdFeB N40H
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.
Sintered NdFeB magnet N42H
N42H
ДСТУ EN 60404-8-1:2022
EN 60404-8-1:2015
Permanent magnets
Sintered anisotropic NdFeB permanent magnet N42H (Eclipse Magnetics grade table): Br >= 1.30 T, HcJ >= 1353 kA/m, (BH)max >= 318 kJ/m^3 (minimum values), maximum operating temperature about 120 °C.
NdFeB N42H
Permanent magnets
Properties, analogues, sources, notes and hardness need a paid account.